Polymer Property : Tensile Strength, Yield = 4460 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.8 MPa
4460 psi
Crosshead speed - 2"min.; ASTM D638
LyondellBasell Alathon® M6138 High Density Polyethylene
ApplicationsALATHON M 6138, formerly known as XM 6138, is a high density polyethylene resin for use in injection molding applications. This resin exhibits good impact resistance and high stiffness...