Polymer Property : Tensile Strength, Yield = 4496 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.00 MPa
4496 psi
At 50 mm/min; ISO 527-2
Borealis BorECO™ BA212E Polypropylene Block Copolymer for Non-Pressure Pipes
BorECO BA212E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high stiffness and impact strength.BorECO BA212E is recommended for solid wall and structured wal..