Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.310 MPa

@Strain 100 %
45.0 psi

@Strain 100 %
ASTM D412
Multibase Multi-Flex® A 1540 Natural TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go..