Polymer Property : Tensile Strength, Yield = 4540 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.3 MPa
4540 psi
ASTM-D638
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade
Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®..
Tensile Strength, Yield 31.3 MPa
4540 psi
ASTM D638
Spartech Royalite R632M Carbon Black Filled ABS/PVC Resin
Data provided by the manufacturer. This static-conductive material is UL®-listed and meets minimum static-decay requirements outlined in MIL-B-1705B and NFPA Code 56A specifications.