Polymer Property : Tensile Strength, Yield = 4580 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.6 MPa
4580 psi
Silon Tabond 5010 Adhesive Resin
Tabond 5010 is a a chemically modified Polypropylene. This grade is for sheets and bottles composed of Polypropylene (PP) and EVOH or PA.Characteristics: • Strong adhesion to PA / PP and EVOH /..
Tensile Strength, Yield 31.6 MPa

@Temperature 23.0 °C
4580 psi

@Temperature 73.4 °F
Molded and tested under D410, 50 mm/min; ASTM D638
Ineos H03G-01 Polypropylene Homopolymer
This is a homopolymer designed for tenter frame BOPP processing and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsFood packagingOverwrap..