Mechanical Properties Metric English Comments
Tensile Strength, Yield 427 - 469 MPa
62000 - 68000 psi
0.2% offset
Eagle Brass 151 ZHC® COPPER, Spring
Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c..
Tensile Strength, Yield 365 - 469 MPa
53000 - 68000 psi
0.2% offset
Eagle Brass 194 HSM® Copper, Hard
High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl..
Tensile Strength, Yield 414 - 469 MPa
60000 - 68000 psi
0.2% offset
Eagle Brass 210 Gilding Metal, Extra Spring
CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi..
Tensile Strength, Yield 324 - 469 MPa
47000 - 68000 psi
0.2% offset
Eagle Brass 510 Phosphor Bronzes 5% A, 1/2 Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Tensile Strength, Yield 241 - 469 MPa
35000 - 68000 psi
Chicago Extruded Metals BioBrass® UNS C64200 Aluminum Bronze
Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Ext..