Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.51 MPa

@Temperature 23.0 °C
4715 psi

@Temperature 73.4 °F
ASTM D638
Ineos H02G-00 Polypropylene Homopolymer
This is a low melt flow rate general purpose homopolymer polypropylene. This grade is designed to meet the processing and physical property requirements of sheet, film, and profile extrusion applic..