Tensile Strength, Yield 48.26 - 55.16 MPa
7000 - 8000 psi
ASTM D638
Ex-Tech Plastics VersaTech™ RPET Packaging Polymer
Primarily used for consumer packaging, VersaTech RPET delivers on excellent clarity and high gloss, while providing good impact and tear resistance properties that are demanded in today’s retail en..