Mechanical Properties Metric English Comments
Tensile Strength, Yield 495 MPa

@Strain 0.200 %,
Temperature 540 °C
71800 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes 214® alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Yield 495 MPa

@Strain 0.200 %
71800 psi

@Strain 0.200 %
Haynes 214® alloy, sheet, 1000 hours exposure at 870°C (1600°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Yield 495 MPa

@Strain 0.200 %
71800 psi

@Strain 0.200 %
Haynes 230® alloy, 30% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Tensile Strength, Yield 495 MPa

@Strain 0.200 %
71800 psi

@Strain 0.200 %
Haynes 25 alloy, room temperature after 20% cold reduction, 1175°C anneal for 5 minutes
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 495 MPa

@Strain 0.200 %
71800 psi

@Strain 0.200 %
Haynes 25 alloy, room temperature sheet after 100 hours of 870°C exposure
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 495 MPa

@Strain 0.200 %
71800 psi

@Strain 0.200 %
Haynes 230® alloy, 50% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..