Polymer Property : Tensile Strength, Yield = 5.18 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 5.18 MPa
>= 751 psi
Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 5407 Nitrile Rubber
General purpose Nitrile; Peroxide curedInformation provided by Seals Eastern, Inc.