Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.32 MPa | 771 psi | @100% Elongation; ASTM D1414 |
Greene Tweed FPD Blueâ„¢ 707 Fluoroelastomer Specifically developed for flat panel display CVD and dry plasma etch equipment where seal reliability and minimal contamination are essential, FPD Blueâ„¢ 707 fluoroelastomer provides excellent .. |