Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.39 MPa | 782 psi | ASTM D412 |
Polymax® Maxelast® D6755 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Strength, Yield | 5.39 MPa | 782 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® S385A Thermoplastic Polyurethane Type: Estane® S385A is a Shore 85A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Information Provi.. |
|||
Tensile Strength, Yield | 5.39 MPa | 782 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® X-585A-31 Thermoplastic Polyurethane Type: Estane® X585A-31 is a Shore 95A, polyester grade without lubricant thermoplastic polyurethane (TPU). USP Class VI Certified.Uses: Extrusion, Film Blowing.Information Provided by The Lubrizol.. |
|||
Tensile Strength, Yield | 5.39 MPa | 782 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® CR185A Thermoplastic Polyurethane Type: Estane® CR185A is a Shore 85A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Tensile Strength, Yield | 5.39 MPa | 782 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® CS185A Thermoplastic Polyurethane Type: Estane® CS185A is a Shore 85A, polyester grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Tensile Strength, Yield | 5.39 MPa | 782 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 8048N Thermoplastic Elastomer Elastocon® 8048N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8048N is FDA compliant and well suited.. |
|||
Tensile Strength, Yield | 5.39 MPa | 782 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® T865A Thermoplastic Polyurethane Type: Estane® T865A is a Shore 71A, polyester grade, plasticized low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Corporation |