Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.54 MPa | 804 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 2840 Thermoplastic Elastomer Elastocon® 2840 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2840 is FDA compliant and well suited for cons.. |