Tensile Strength, Yield 5.55 MPa
805 psi
200°C for 1,000 hrs
Fujipoly Industries Sarcon® 45Q Thin-Film QR
Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov..