Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.625 MPa
815.8 psi
-25% change after 70 hours @ 200°C; ASTM D412
Precision Polymer Engineering S80B Silicone Rubber
Black Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and ..
Tensile Strength, Yield 5.625 MPa
815.8 psi
-25% change after 70 hours @ 200°C; ASTM D412
Precision Polymer Engineering S80G Silicone Rubber
Green Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and ..
Tensile Strength, Yield 5.625 MPa
815.8 psi
-25% change after 70 hours @ 200°C; ASTM D412
Precision Polymer Engineering S80Y Silicone Rubber
Yellow Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and..
Tensile Strength, Yield 5.625 MPa
815.8 psi
-25% change after 70 hours @ 200°C; ASTM D412
Precision Polymer Engineering S80Z Silicone Rubber
Grey Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and l..