Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 35.2 MPa | 5110 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ HTX Ultra LA426 Gray 2382 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert.. |
|||
Tensile Strength, Yield | 35.2 MPa | 5110 psi | ASTM D638 |
Dow H110-02N Polypropylene Homopolymer Resin OverviewContains a nucleating agentHigh clarityGood melt strengthComplies with U.S. FDA 21 CFR 177.1520 (c)3.2a, Canadian HPFB No ObjectionDOW H110-02N Polypropylene Resin is intended for use in ext.. |
|||
Tensile Strength, Yield | 35.2 MPa | 5110 psi | ASTM D638 |
Dow NRD6-589 Polypropylene Random Copolymer Resin DOW NRD6-589 Polypropylene Resin is intended for use in injection molding applications. It offers excellent balance of impact and stiffness.Consistent processabilityGood stiffness/impact balanceGoo.. |
|||
Tensile Strength, Yield | 35.2 MPa | 5110 psi | ASTM Data |
Dow Prevail® 3050 ABS + Polyurethane PREVAIL® 3050 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used .. |
|||
Tensile Strength, Yield | 35.2 MPa | 5110 psi | 2 in/min (50 mm/min); ASTM D638 |
Bapolene® 4071 Polypropylene, Fiber/Injection Grade Bapolene PP4071 is a high flow PP homopolymer for staple and continuous filament applications as well as general purpose injection molding. This resin exhibits good melt and thermal stability.Appli.. |
|||
Tensile Strength, Yield | 35.2 MPa | 5110 psi | ASTM D412 |
ACC EP RAP 60 EPI Engineered Polymers Aliphatic Polyurea EP RAP 60 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC, coating (silicone optional) developed for UV stable (colorfast) polyurea flooring applic.. |
|||
Tensile Strength, Yield | 35.2 MPa | 5110 psi | ASTM D638 |
Dow H110-02NZ Polypropylene Homopolymer Resin OverviewContains a nucleating agentGood melt strengthComplies with U.S. FDA 21 CFR 177.1520 (c)3.2aDOW H110-02NZ Polypropylene Resin is intended for use in extrusion and thermoforming processes in o.. |
|||
Tensile Strength, Yield | 35.2 MPa | 5110 psi | ASTM D638 |
Braskem INSPIRE™ 222 Performance Polypropylene Polymer INSPIRE™ 222 Performance Polymer is intended for use in extrusion and thermoforming processes. It is especially suited in applications requiring excellent clarity and good stiffness.Contains a nuc.. |