Polymer Property : Tensile Strength, Yield = 53.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 53.7 MPa

@Thickness 3.20 mm
7790 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUCEL FW700N Modified POM, Friction Resistance, Abrasion Resistance
Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical