Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.65 MPa
530 psi
at 100%; ASTM D412
1074A Polyurethane-based Biomedical Elastomer
Tensile Strength, Yield 3.65 MPa
530 psi
@100% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 504 Perfluoroelastomer
Greene Tweeds Chemraz® 504, a 65 Shore A hardness perfluoroelastomer, provides an extremely broad range of chemical resistance and is perfect for services with low pressures and/or low temperatur..
Tensile Strength, Yield 3.65 MPa

@Strain 300 %
530 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® IT 38-046E Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerTranslucentApplications:FDA (Food Contact)Market:Consumer GoodsProcessing Method:ExtrusionPolyOne First ChoiceDisclaimer: A thermoplastic..