Polymer Property : Tensile Strength, Yield = 54.6 MPa
Polymer Property :
Tensile Strength, Yield =
54.6 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
54.6
MPa
7920
psi
chs 2.0 in/min; ASTM D638
Diamond Polymers NPP 808 C3 TDS Polycarbonate Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.