Polymer Property : Tensile Strength, Yield = 540 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 540 MPa

@Strain 0.200 %,
Temperature 540 °C
78300 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes 242® alloy, bar and rings, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Yield 540 MPa

@Strain 0.200 %,
Temperature 540 °C
78300 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes 25 alloy, cold worked sheet, 10% cold reduction
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 540 MPa

@Strain 0.200 %,
Temperature 540 °C
78300 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes 263® alloy, cold rolled sheet, solution treated and aged
Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle..
Tensile Strength, Yield 540 - 610 MPa

@Strain 0.200 %
78300 - 88500 psi

@Strain 0.200 %
CLAL-MSX DECLAFOR® 1015 TD3 Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Tensile Strength, Yield 540 - 650 MPa

@Strain 0.200 %
78300 - 94300 psi

@Strain 0.200 %
CLAL-MSX DECLAFOR® 1015 TF Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Tensile Strength, Yield 540 - 590 MPa
78300 - 85600 psi
T direction
ArcelorMittal Speed 35-510 Electrical Steel
Properties: The iCARe™ Speed product family comes with guaranted losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 540 MPa

@Strain 0.200 %
78300 psi

@Strain 0.200 %
Haynes 25 alloy, room temperature after 15% cold reduction, 1120°C anneal for 5 minutes
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall..