Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 37.93 MPa | 5501 psi | ASTM D638 |
Lucent Polymers ABS-45T Acrylonitrile Butadiene Styrene, High Impact Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |