Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 496 - 565 MPa @Strain 0.200 % |
72000 - 82000 psi @Strain 0.200 % |
Plate and Rounds |
IBC Advanced Alloys C18150 Chrome Copper Zirconium Alloy, TL06 Temper C18150 Chrome Copper Zirconium is recommended for spot and seam welding cold and hot-rolled steel, stainless steel and low conductivity brass and bronze. C18150 Chrome Copper Zirconium Alloy is typi.. |
|||
Tensile Strength, Yield | 490 - 565 MPa | 71000 - 82000 psi | 0.2% offset |
Eagle Brass 706 Copper Nickel 10%, Extra Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Tensile Strength, Yield | 476 - 565 MPa | 69000 - 82000 psi | 0.2% offset |
Eagle Brass 752 Nickel Silver 18%, 3/4 Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |