Mechanical Properties Metric English Comments
Tensile Strength, Yield 39.4 MPa
5710 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion LR610 white 1046 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 39.4 MPa
5710 psi
Type I, 51 mm/min; ASTM D638
PolyOne Nanoblend™ LST 5501 Polypropylene, Unspecified (PP, Unspecified)
Nanoblend compounds, formerly known as Maxxam LST, are LIGHT, STIFF AND TOUGH. Using nanoclay technology, these compounds deliver a combination of high stiffness and impact resistance to meet demand..