Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 39.57 MPa | 5739 psi | ASTM D412 |
Lubrizol Advanced Materials Pearlthane® 12T92E Thermoplastic Polyurethane Elastomer PEARLTHANE® 12T92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and low temperature performance. This gra.. |