Polymer Property : Tensile Strength, Yield = 595 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.10 MPa
595 psi
200%, post cured- 4 hours at 200°C; ASTM D412
Multibase SILASTIC® Q7-4840 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tensile Strength, Yield 4.10 MPa
595 psi
ASTM D412
Polymax® Maxelast® P2950T TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 4.10 MPa
595 psi
ASTM D412
Polymax® Maxelast® P3740 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 4.10 MPa
595 psi
M100
3M Dyneon™ Fluorel™ FC-2176 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Good general purpose grade with good ..
Tensile Strength, Yield 4.10 MPa
595 psi
At 100% elongation, across flow; ASTM D412
Advanced Elastomer Systems VistaFlex® 715-B Thermoplastic Rubber  (discontinued **)
Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f..
Tensile Strength, Yield 4.10 MPa

@Strain 100 %
595 psi

@Strain 100 %
Daikin DAI-EL G-501NK Fluoroelastomer Terpolymer, Diamine Curable Grade, 68% Fluorine Content
Features: Good mechanical characteristics.Information provided by Daikin Industries.
Tensile Strength, Yield 4.10 MPa

@Strain 100 %
595 psi

@Strain 100 %
Daikin DAI-EL G-575 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 70% Fluorine Content
Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Low permeability to gasoline and a..
Tensile Strength, Yield 4.10 MPa
595 psi
chs 20 in/min; ASTM D638
Diamond Polymers Softflex® 4550
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 4.10 MPa
595 psi
508 mm/min; ASTM D638
Dow Engage® 8003 Polyolefin Elastomer
Description: Engage® 8003 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide variety of general purpose thermoplastic elastomer ..
Tensile Strength, Yield 4.10 MPa
595 psi
cured 72 hrs @ RT
ACC QM 245 QSI Quantum Silicones 45 Durometer Addition Cure Moldmaking Material
QM 245 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for th..
Tensile Strength, Yield 4.10 MPa
595 psi
M100
3M Dyneon™ Fluorel™ FC-2211 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp..