Polymer Property : Tensile Strength, Yield = 6.40 MPa
Polymer Property :
Tensile Strength, Yield =
6.40 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
6.40
MPa
928
psi
ASTM D412
Vicone High Performance Rubber VicoSilâ„¢ 0591EK-CL High Performance Silicone Rubber