Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.80 MPa
986 psi
ASTM D412
Polymax® Maxelast® F02-137D TPE, Halogen Free Extrusion Grade
Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to..
Tensile Strength, Yield 6.80 MPa
986 psi
M100
3M Dyneon™ Fluorel™ FE-5840Q Fluoroelastomer VF2 + HFP + TFE Terpolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 70.1%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c..
Tensile Strength, Yield 6.80 MPa
986 psi
Elastic Limit
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy
Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor..
Tensile Strength, Yield 6.80 MPa
986 psi
ASTM D412
ExxonMobil Vistamaxx™ 3980FL Propylene-based Elastomer - High Purity, Low Gel
Product Description: Vistamaxx 3980FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced us..
Tensile Strength, Yield 6.80 MPa
986 psi
Dow AFFINITY™ PL 1840 Polyolefin Plastomer
AFFINITY® PL 1840 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide blown film products with low temperature sealability, excellent puncture resistance, outstanding blown f..