Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.33 MPa | 628 psi | 60°C for 500 hrs with 95% RH |
Fujipoly Industries Sarcon® 30Q Thin-Film QR Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Tensile Strength, Yield | 4.33 MPa | 628 psi | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 30U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |