Mechanical Properties Metric English Comments
Tensile Strength, Yield 630 MPa
91400 psi
0.2%; EN 10002-1
Plansee Cu-MoCu-Cu Laminate
A high performance, three-layer composite.Characteristics:High thermal conductivityLow thermal expansionIdeal for heat dissipation applications related to: IGBT modules, RF packages, and LED chips, ..
Tensile Strength, Yield 630 MPa

@Strain 0.200 %
91400 psi

@Strain 0.200 %
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Yield 630 MPa

@Strain 0.200 %,
Temperature 425 °C
91400 psi

@Strain 0.200 %,
Temperature 797 °F
Precipitation Hardened prior to test
Special Metals MONEL® Alloy K-500
A precipitation-hardenable nickel-copper alloy that combines the corrosion resistance of MONEL alloy 400 with greater strength and hardness. It also has low permeability and is nonmagnetic to under..
Tensile Strength, Yield 630 - 780 MPa

@Strain 0.200 %
91400 - 113000 psi

@Strain 0.200 %
CLAL-MSX DECLAFOR® 1015 TDX Rod quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Tensile Strength, Yield 630 MPa

@Strain 0.200 %,
Temperature 205 °C
91400 psi

@Strain 0.200 %,
Temperature 401 °F
Haynes 242® alloy, hot rolled plate, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal..
Tensile Strength, Yield 630 MPa

@Strain 0.200 %
91400 psi

@Strain 0.200 %
Haynes 25 alloy, room temperature after 15% cold reduction, 1065°C anneal for 5 minutes
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall..