Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 42.2 - 43.8 MPa | 6120 - 6350 psi | ASTM D638M |
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC -2 DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons.. |