Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 64.7 MPa | 9390 psi | ASTM D638 |
Lendell Parapet PMMA, High Flow |
|||
Tensile Strength, Yield | 64.7 MPa @Thickness 3.20 mm |
9390 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUCON PS4200 ABS+CF Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Good Dimensional Stability, Low WarpageApplication: IC TrayCAS No. 9003-56-9, 12001-26-2 and 7440-44-0Information provided by LG Ch.. |
|||
Tensile Strength, Yield | 64.7 MPa @Thickness 3.20 mm |
9390 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose Feature: Injection Molding, ABS+GF10%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 64.7 MPa | 9380 psi | ASTM D412 |
C.O.I.M. LARIPUR® LPR6520 Standard Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |