Polymer Property : Tensile Strength, Yield = 64500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 445 MPa

@Strain 0.200 %
64500 psi

@Strain 0.200 %
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Yield 445 MPa

@Strain 0.200 %
64500 psi

@Strain 0.200 %
Haynes 188 alloy, plate at RT after 8000 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Yield 445 MPa

@Strain 0.200 %
64500 psi

@Strain 0.200 %
Haynes 230® alloy, 20% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Tensile Strength, Yield 445 MPa

@Temperature 760 °C
64500 psi

@Temperature 1400 °F
Haynes Hastelloy® W alloy, gas tungsten arc welds, aged 1000 hours at 650°C (1200°F)
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica..
Tensile Strength, Yield 445 MPa

@Strain 0.200 %
64500 psi

@Strain 0.200 %
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..