Polymer Property : Tensile Strength, Yield = 65.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.2 MPa

@Strain 0.200 %
9460 psi

@Strain 0.200 %
Malvern Minerals Epoxy with 50% Novacite® Daper Quartz Filler
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..