Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.48 MPa
650 psi
at 200%, no post cure- press cured for 5 minutes; ASTM D412
Multibase SILASTIC® 7-6860 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tensile Strength, Yield 4.48 MPa
650 psi
ASTM D412
Polymax® Maxelast® A9755 TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Tensile Strength, Yield 4.48 MPa
650 psi
@50% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® SD625 Perfluoroelastomer
Chemraz® SD625, a black-colored perfluoroelastomer, offers the broadest chemical resistance of any elastomer, combining the resilience and sealing force of an elastomer with chemical resistance a..
Tensile Strength, Yield 4.48 MPa
650 psi
Elastic; ASTM D412
Multibase Multi-Flex® A 2599 TPE Thermoplastic Elastomer
This material bonds to polypropylene. Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame Retardant Flexibility, GoodHeat StabilizedOzone ResistantPr..
Tensile Strength, Yield 4.48 MPa
650 psi
100%; ASTM D412
Teknor Apex APEX® 3070-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin..
Tensile Strength, Yield >= 4.48 MPa
>= 650 psi
Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 5803 Fluoro-silicone
Fluoro-siliconeInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 4.48 MPa
650 psi
100%; ASTM D412
Teknor Apex APEX® 3301-65 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
Tensile Strength, Yield 4.48 MPa
650 psi
Master Bond Mastersil 803 One component Room Temperature Curing Non- Corrosive Silicone
Master Bond MasterSil 803 is a ready-to-use, one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. This material is a clea..
Tensile Strength, Yield 4.48 MPa
650 psi
Flatwise Tensile
Hexcel® Redux® 609 (0.04 psf) Adhesive film for bonding metallic and composite components
Redux 609 is a 250°F curing modified epoxy film adhesive containing a cottom scrim for easy handling and glue-line thickness control. It is available at standard areal weights of 0.06 psf and 0.04 ..
Tensile Strength, Yield 4.48 MPa

@Strain 300 %
650 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® IT 62-002 BLACK 2001 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Over-Molding GradeUV StabilizedApplications: Multi-PurposeProcessing Method: Injection MoldingInformation provided by PolyOne Corporation
Tensile Strength, Yield 4.48 MPa

@Strain 300 %
650 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® RT-3860E Thermoplastic Elastomer - SBC  (discontinued **)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..