Polymer Property : Tensile Strength, Yield = 678 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 678 MPa

@Strain 0.200 %
98300 psi

@Strain 0.200 %
Haynes Hastelloy® S alloy, gas tungsten arc welded, aged 1300 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Yield 678 MPa

@Strain 0.200 %
98300 psi

@Strain 0.200 %
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 34.5% Cold Work
AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze..