Polymer Property : Tensile Strength, Yield = 7.30 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.30 MPa
1060 psi
M100
3M Dyneon™ Fluorel™ FE-5623Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c..
Tensile Strength, Yield 7.30 MPa
1060 psi
M100
3M Dyneon™ Fluorel™ FC-2178 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp..
Tensile Strength, Yield 7.30 MPa

@Strain 300 %
1060 psi

@Strain 300 %
ISO 527-1/-2
Covestro Desmopan® KU 2-8671 Polyurethane
As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Tensile Strength, Yield 7.30 MPa
1060 psi
Dow DOWLEX™ 2517 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2517 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and low temperature properties with excellent f..
Tensile Strength, Yield 7.30 MPa
1060 psi
Dow Primacor® 3460 Ethylene Acrylic Acid (EAA)
PRIMACOR® 3460 polymer containing 9.5% comonomer is a heat seal coating for high speed packaging applications where low temperature processing is necessary for minimal taste and odor effects. It is..
Tensile Strength, Yield 7.30 - 42.0 MPa
1060 - 6090 psi
Average value: 15.4 MPa Grade Count:68
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..