Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 - 71.0 MPa
8990 - 10300 psi
ISO.527 DN.53455
Polimersan Plastics POLIPOM® (POM)
POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional..
Tensile Strength, Yield 62.0 - 71.0 MPa
8990 - 10300 psi
ISO.527 DN.53455
Polimersan Plastics POLIPOM® (POM)
POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional..