Polymer Property : Tensile Strength, Yield = 7103 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.97 MPa
7103 psi
ASTM D638
Lucent Polymers PC/PBT-1420IM Polycarbonate+PBT, Superior Cold Temp Impact, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.