Polymer Property : Tensile Strength, Yield = 7107 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 49.00 MPa
7107 psi
ASTM D638
I. Stern N2380 High Heat Crystal Polystyrene
Features:High Molecular WeightExcellent Optical PropertiesApplicationsOPSFoamed TraysThick Walled Injection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. St..