Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 717 MPa @Strain 0.200 % |
104000 psi @Strain 0.200 % |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 2 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Tensile Strength, Yield | 717 MPa @Strain 0.200 %, Temperature -73.3 °C |
104000 psi @Strain 0.200 %, Temperature -100 °F |
|
Carlson Nitronic® 33® Austenitic Stainless Steel General DescriptionNitronic 33 is a nitrogen-strengthened austenitic stainless steel that combines high yield strength with excellent toughness and ductility. It’s magnetic permeability remains v.. |
|||
Tensile Strength, Yield | 717 MPa @Strain 0.200 %, Temperature -73.0 °C |
104000 psi @Strain 0.200 %, Temperature -99.4 °F |
|
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 10% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |