Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 72.60 MPa | 10530 psi | ASTM D638 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 72.60 MPa | 10530 psi | ASTM D638 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 72.60 MPa | 10530 psi | ASTM D638 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 72.60 MPa | 10530 psi | ASTM D638 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 72.60 MPa | 10530 psi | ASTM D638 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 72.60 MPa | 10530 psi | ASTM D638 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |