Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 74.1 MPa | 10700 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers ABSPC 9901GF20 Injection Molding Grade, 20% Glass Filled Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |