Polymer Property : Tensile Strength, Yield = 76000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 524 MPa

@Strain 0.200 %
76000 psi

@Strain 0.200 %
Haynes Ultimet® alloy, 12.7-50.8 mm bar
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Tensile Strength, Yield 524 MPa

@Strain 0.200 %
76000 psi

@Strain 0.200 %
Haynes Hastelloy® C-22® alloy, GTAW weld, C-22 base metal, C-22 weld metal
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Yield >= 524 MPa
>= 76000 psi
0.2% offset
Eagle Brass 706 Copper Nickel 10%, Spring
706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to..
Tensile Strength, Yield 524 MPa
76000 psi
CMW® THERMKON® 83 Tungsten Copper parts
For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc.
Tensile Strength, Yield 524 MPa

@Strain 0.200 %,
Temperature 566 °C
76000 psi

@Strain 0.200 %,
Temperature 1050 °F
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Tensile Strength, Yield 524 MPa

@Strain 0.200 %
76000 psi

@Strain 0.200 %
Haynes Hastelloy® C-22® alloy, all-weld metal, GTAW
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..