Polymer Property : Tensile Strength, Yield = 77.57 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 77.57 MPa
11250 psi
ASTM D638
Spartech Polycast Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Tensile Strength, Yield 77.57 MPa
11250 psi
ASTM D638
Spartech Polycast Poly 76 (Mil-P-8184) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Tensile Strength, Yield 77.57 MPa
11250 psi
ASTM D638
Spartech Polycast Poly 84 (Mil-P-8184) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Tensile Strength, Yield 77.57 MPa
11250 psi
ASTM D638
Spartech Polycast Poly 900 (DTD-5592-UK) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Tensile Strength, Yield 77.57 MPa
11250 psi
ASTM D638
Spartech Polycast Poly II (Mil-P-5425) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Tensile Strength, Yield 77.57 MPa
11250 psi
ASTM D638
Spartech Polycast UF3 Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Tensile Strength, Yield 77.57 MPa
11250 psi
ASTM D638
Spartech Polycast UF4 Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Tensile Strength, Yield 77.57 MPa
11250 psi
ASTM D638
Spartech Polycast UF96 Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Tensile Strength, Yield 77.57 MPa
11250 psi
ASTM D638
Spartech Polycast UVT (Ultra-Violet Transmitting) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.