Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 531 MPa | 77000 psi | |
Niagara LaSalle 1045 Cold Finished Steel Bar This medium carbon steel is used for heat treating (quenching and tempering). Although it has only a fair response to conventional quenching, it is widely used where requirements are not too stringe.. |
|||
Tensile Strength, Yield | 531 MPa @Temperature 23.9 °C |
77000 psi @Temperature 75.0 °F |
0° Direction, Dry; Press Cure, 16min, 300°F; ASTM D638 |
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 3K PW Reinforced Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring .. |
|||
Tensile Strength, Yield | 531 MPa @Strain 0.200 % |
77000 psi @Strain 0.200 % |
|
Haynes Ultimet® alloy, aged 1000 hours at 538°C (1000°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 531 MPa @Strain 0.200 % |
77000 psi @Strain 0.200 % |
|
Haynes Ultimet® alloy, aged 1000 hours at 760°C (1400°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |