Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 53.3 MPa | 7730 psi | ASTM D1458 |
Fujipoly Industries Sarcon® 15GHR Thin-Film GHR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Tensile Strength, Yield | 53.3 MPa | 7730 psi | 60°C for 500 hrs with 95% RH |
Fujipoly Industries Sarcon® 30GSR Thin-Film GSR Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of.. |