Polymer Property : Tensile Strength, Yield = 793 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 793 MPa

@Temperature 899 °C
115000 psi

@Temperature 1650 °F
oil quench, tempered at 1200°F
Latrobe Nitralloy® N™ VAC-ARC Premium Nitriding Steel
NITRALLOY N is an age hardenable nitriding steel. The age hardening capability of the alloy permits the core strength to be developed while the surface is being nitrided. VAC-ARC remelting is employ..
Tensile Strength, Yield 793 - 1172 MPa
115000 - 170000 psi
Materion Beryllium Nickel Strip - Alloy 360 1/2 Hard
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0.7Formability Ratio (bad Way)..
Tensile Strength, Yield 793 - 1030 MPa

@Strain 0.200 %
115000 - 150000 psi

@Strain 0.200 %
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished and Aged Rod and Bar
Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished and Aged Rod and Bar specifically. Other property values are typical of aged DURANIC..
Tensile Strength, Yield 793 - 931 MPa

@Strain 0.200 %,
Thickness >=25.4 mm
115000 - 135000 psi

@Strain 0.200 %,
Thickness >=1.00 in
Turned Bars
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar
Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect..
Tensile Strength, Yield 793 MPa

@Strain 0.200 %
115000 psi

@Strain 0.200 %
Annealed
Universal Wire Works 5Al-2.5Sn (AMS 4953) Titanium Alloy Filler Metal
Universal Ti 5Al-2.5Sn titanium alloy is easily joined with the gas tungsten arc, gas metal arc or resistance welding processes. 100% joint efficiency can be obtained provided proper shielding proce..
Tensile Strength, Yield >= 793 MPa
>= 115000 psi
0.2% offset
Eagle Brass 770 Nickel Silver 18%, Extra Spring
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
Tensile Strength, Yield 793 MPa

@Strain 0.200 %
115000 psi

@Strain 0.200 %
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 35% Cold Worked
Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro..
Tensile Strength, Yield 793 MPa
115000 psi
0.2% Offset
ATI Allvac® 6-4ELI Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
Data provided by Allvac.Applications: Applications requiring excellent fracture toughness and fatigue strength; aircraft, structural components, biomedical.
Tensile Strength, Yield 793 MPa

@Strain 0.200 %
115000 psi

@Strain 0.200 %
ATI Allvac® 6-7 UNS R56700 Titanium Alloy
Uses: Biomedical implants. Femoral hip stems, fracture fixation plates, spinal components, fasteners, nails, rods, screws, wire.Property values are for samples in the metallurgical condition: 1300°..
Tensile Strength, Yield 793 MPa

@Strain 0.200 %
115000 psi

@Strain 0.200 %
ATI Allvac® Nickelvac® X-750 Nickel Superalloy, Heat Treatment: 982°C (1800°F) + Age
Data provided by Allvac.Applications: Turbine, engine components. Blades, vanes, fasteners, springs, bellows. Extrusion dies, nuclear, heat treating, forming tools.
Tensile Strength, Yield 793 MPa

@Strain 0.200 %
115000 psi

@Strain 0.200 %
ATI Allvac® Rene 41® Nickel Superalloy, Heat Treatment: 1079°C (1975°F) + Age
Data provided by Allvac.Applications: Jet and rocket engines, torque rings, afterburners, and hardware; space shuttle turbo pumps seals.
Tensile Strength, Yield 793 MPa

@Strain 0.200 %,
Temperature 427 °C
115000 psi

@Strain 0.200 %,
Temperature 801 °F
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..