Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.384 MPa | 1216 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7065 Neoprene / Chloroprene General purpose neopreneInformation provided by Seals Eastern, Inc. |