Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 806 MPa @Strain 0.200 % |
117000 psi @Strain 0.200 % |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1149°C (2100°F) 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |