Polymer Property : Tensile Strength, Yield = 8060 psi
Polymer Property :
Tensile Strength, Yield =
8060 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
55.6
MPa
8060
psi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Molding MR900 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne